[quote=BigMace]Well upon further inspection, I have found the inside of the starboard hull to be pretty bad.
It looks like I will have to do nearly the entire upper ~6 inches of the hull for a good portion of the boat... as well as a ~16" diameter area near the bow. The outsides of the hulls do not appear to have any delamination though. Maybe the previous owners only waxed the outside? At least it will make getting away with not seeing the repairs easier.
Ironically, the port hull has just a 4" by 8" area at the bow.
What happens if I inject the epoxy in an area that is not delaminated? I feel like it is sort of a hit and miss game with getting the "feeling" of delamination. I know the crunchy sound is delamination for sure, but how far out around that area should I go?
Thanks,
Mace[/quote]